No.
|
Colour shade
|
|
|
TEMPERATURE
|
|
101
|
white
|
|
|
400
|
|
106
|
Black
|
|
|
400
|
|
104
|
Scarlet
|
|
|
240
|
|
102
|
Deep red
|
|
|
400
|
|
3001
|
Fluorescence Peach red
|
|
|
200
|
|
3002
|
Fluorescence Orange
|
|
|
220
|
|
109
|
Rose red
|
|
|
240
|
|
3007
|
Fluorescence Voilet
|
|
|
300
|
|
103
|
Process Yellow
|
|
|
270
|
|
3003
|
Fluorescence Yellow
|
|
|
220
|
|
107
|
Dark green
|
|
|
300
|
|
3004
|
Fluorescence Green
|
|
|
220
|
|
5011
|
Ultramarins blue
|
|
|
400
|
|
105
|
Bright blue
|
|
|
400
|
|
110
|
Voilet
|
|
|
400
|
|
877C
|
silver
|
|
|
400
|
|
871C
|
Greenish gold
|
|
|
400
|
|
876C
|
red-golden
|
|
|
400
|
|
SP-4
|
Luminous
|
|
|
400
|
|
|
Kerosene
|
|
|
|
|
|
|
|
| Payment Terms︰ | TT |
| Packing︰ | Plastics Can |
| Usage︰ | The bases of silica gel ink is organic silicone polymer,which has good viscosity to the silica gel.It mainly be used to print on rubber keypad,remote control,silica wrist strap,cell phone case,watchband and all kinds of silica products.It is widely be used in car, motorcycle, household electrical appliances, electonic product,toy and medical facilities. |
| Technical Parameter︰ | Curing time:10~15 mins/180℃~250℃ Viscosity:>250dpa.s Fineness:<15μm Solvent:: Odorless kerosene Package:1kg/barrels
|
| Production Advantage ︰ | 1.Colorful,print logo clear and high gloss 2. High flowability makes it easy to operate 3. High-temperature baking does not fade 4. Strong adhesion and long use life 5.can be mutually mixed up to special colour
|
| Use Method︰ | 1.Screen printing ink should be stock in Fridge(below 0℃),make sure it is not be ossified before use. 2.Kerosene can be used to dilute the screen printing ink.As it includes solvent in the used ink,so it can be fill into the barrel again.So you’d better dilute the ink according to your need.When the screen frame was plugged up,the toluol or gas can be used to wipe it. 3.Before printing,please wash the parting agent and oil dirt of objects with water,then drying it with dust gun. 4.After printing,put the objets in the room about 15 mins,then dry it under 200℃ about 10 to 20 mins.
|
|
|
|